R-TECH Materials gains UKAS accreditation for metallography tests

R-TECH Materials have successfully obtained UKAS accreditation for the following metallography tests:

  • Depth of case hardening
  • Decarburisation depth by both the microscopical and micro indentation methods
  • Detecting detrimental intermetallic phases
  • Average grain size using the intercept method
  • Volume fraction by systematic manual point count

With a team of highly experienced metallurgists, R-TECH are also able to offer consultancy support alongside these metallurgical tests for the development of specific products or to investigate materials issues.